• High light non-trace injection mold and molding technology Jul 23, 2021
    Highlights are typical of non-mark injection molding highlights, but not all of the non-mark injection. We have been making high-light molds for several years, mainly for the external decorative parts of home appliance products, such as front panels, decorative pieces, etc., but every time we have encountered the same problem, that is, we cannot solve the fusion mark, shrinkage mark and other...
  • Injection molding defects │ how to solve the high-gloss product surface fog? Jul 23, 2021
    Highlight products for injection molding enterprises is really a difficult problem to deal with, because it can not hide external defects, even the dust in the workshop will cause different degrees of product defects, such as troma, pitting, contamination, etc., so the environment is also one of the key factors affecting this kind of products. The white fog on the surface of the product is wh...
  • Something about the mold distance tension mechanism failure Jul 30, 2021
    Pendulum hook, buckle and other distance tension mechanism is generally used in the fixed mold core pulling or some secondary release of the mold, because this kind of mechanism is set in pairs on both sides of the mold, its action must be synchronized, that is, the mold at the same time buckle, open the mold to a certain position at the same time decoupling. Once the synchronization is lost, it i...
  • What you can do when you encounter these injection molding machine common failures? Jul 30, 2021
    Even people who have been focused on injection molding for many years also always encounter problems when operating injection molding machines. At this time, how to deal with them is a test of one's experience and technology. The following are 4 points that explain what the sudden failure problem is and how to solve it. 1. the oil pump motor and oil pump start, but no pressure. (1)The pr...
  • Acrylic injection molding process Aug 11, 2021
    Acrylic chemical named poly methyl methacrylate (PMMA). Because PMMA surface hardness is not high, easy to wipe hair, low impact resistance, molding flow performance and other shortcomings, PMMA modification has appeared. Such as methyl methacrylate and styrene, butadiene copolymerization, PMMA and PC blend, etc. The flow generation ratio of PMMA is lower than PS and ABS, and the melt vi...
  • Injection mold cooling lines leakage fault and troubleshooting method Aug 11, 2021
    Injection mold cooling line leakage is a common occurrence. There are many reasons, mainly from the following aspects: 1. Most occurs at the joint of the mold cooling lines. If leakage is found, the sealing belt should be wound on the thread of the pipe connector, and then tightened. 2. Due to long-term molding conditions, the o-ring in the mold will be damaged, and the O-shaped o-ring is eas...
  • Injection mold maintenance skills Aug 11, 2021
    In order to determine the mold damage state and repair measures. Processing enterprises should be in the injection molding machine, under the normal operation of the mold, test the performance of the mold, and the final molded plastic parts size measurement, through these information can determine the existing state of the mold, find out the cavity, core, cooling system and parting surface da...
  • Automobile sensor bracket precision mold design case Aug 12, 2021
    1. Product analysis: This case is for a bracket on the sensor of a car. The precision requirement is very high, the material is POM, the product is very small, the longest size is 38mm, and the metal insert (copper sheet) should be put when injection molding, and the deformation amount is very small, see Figure below. The upper and lower two holes of this product is not concentricity is ...
1 ... 26 27 28 29

A total of 29 pages

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Home

Services

about

contact