Short shot
Nov 20, 2019
We are going to talk about one of the most common problem during mould trial--short shot. The factor are as below: 1. It means that the cavity is not completely filled, caused the plastic parts incomplete; 2. The mold venting is not good; 3. The section of gate and runner is too small and long, The melt pressure loses too much during the flow; 4. The thin wall is not thick enough; 5. There is no c...