• What's welding line? Jan 10, 2020
    Welding Line is refers to the slim line disappear in which the plastic raw material melting and collecting. Why it happens? 1. Insufficient liquidity of melting raw materials 2. Have air or volatile component 3. Release agent or colorant 4. Defect of mold design How to improve? 1. Change raw material to better liquidlity 2. Check and improve the air venting, decrease the injection speed 3. Use les...
  • What are the procedures for texture? Jan 16, 2020
    Before, We have talked about the mould texture. There are 7 procedures for mould texture as below: 1.Cleaning the cavity surface 2.Covering the cavity surface which no need to be texture,or painting antiseptic paint on it 3.Drying the antiseptic paint 4.Using degrease cotton to clear the cavity surface which need to be texture, make sure that there's no any impurities and filth to effect texture. ...
  • What are the Four Major Engineering Materials? What's their application? Jan 17, 2020
    Plastic raw materials have many different types.Today we will take about the engineering plastic materials.So what are the Four Major Engineering Materials and what's their applications ? The answer is as follow: 1.ABS, full name is Acrylonitrile Butadiene StyreneAcrylonitrile Butadiene Styrene. It's widely used in machinery, automotive, electronic appliances, instrumentation, textile and construc...
  • Defects analysis of injection molded products - Bubbles Jan 17, 2020
    Bubbles are the phenomenon of small volume or series of pores formed inside the product. A large amount of gas is mixed into the melt and is formed by cooling the melt. 1. Venting system is bad or blocked 2. The cooling system is not setting properly, which makes the material cooling uneven or insufficient. 3. The injection speed is too fast 4. The material temperature is too high, which will caus...
  • Common injection molding product defects and solutions-6 Jan 17, 2020
    Burr the reason: 1.Insufficient clamping force. 2.The injection pressure is too high. 3.Injection speed is too fast. 4.The holding pressure switch is too late. 5.Insufficient mold support. 6.Defect of mold parting surface. 7.The melt temperature is too high. 8.Low viscosity. Solution: 1.Reduce filling speed or holding pressure. 2.Improve the clamping force. 3. Change the position or method of hold...
  • Two-color mold design and injection tips
    Two-color mold design and injection tips Mar 20, 2020
    1. The water circiuts of the cavities and cores is designed as full as possible and balanced. 2. After the cavity rotates 180 ° from the center, it must match the core. 3. Usually, injecting the hard rubber part first, and then the soft rubber part, because soft rubber is easy to deform. 4. The nozzle of the three-plate mold should preferably be designed to automatically demolding. Special attenti...
  • What is the extrusion mold? Mar 27, 2020
    Extrusion mold is a kind of molding mold, but its way of molding is extrusion.  It is widely used in aluminum shaped structures and also in plastic parts.  In the front of the extruder, used to make pipe or profile. In short, a mold is a tool used to form an object. The tool is made up of various parts. Different molds are made up of different parts.  It mainly processes product by ...
  • Tips for injection molding of nylon cable ties
    Tips for injection molding of nylon cable ties Apr 10, 2020
    1. Pay attention to mold temperature If the lower temperature of the heat-resistant and abrasion-resistant nylon cable ties in the production, the faster the material cooling rate in the mold cavity, so that it can greatly shorten the take-out time of the product and improve the efficiency of the molding operation. However, if the temperature is too low, it will easily cause the appearance of the ...
1 ... 17 18 19 20 21 ... 28

A total of 28 pages

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Home

Services

about

contact