• The short shot checkpoints Jun 28, 2019
    The short shot checkpoints As mentioned that, when the melt is cooled down without filling the mold cavity, or the melt does not fill completely after running into the cavity, it is called the short shot injection molding. We analyse the reasons of short shot. So today let’s discuss how to improve the insufficient injection. Here lists short shot checkpoints: 1) Improper control of process conditi...
  • There are undercuts around products'4 corner,should we make lifter or slider? Jul 08, 2019
    As we know, During mold designing, If the product has inner undercut, we usually make lifter, If has outside undercut, we will make slider, But If it has undercut around the 4 corner, and couldn't be forced demoulding, what should we do? As below picture, should we make lifter or slider? 1.  Design Analysis If so, first we will think about to make lifter, but after analyze, If make lifter the...
  • The Classification of Plastic Raw Material Jul 19, 2019
    The phrase plastic is familiar to us, but most people don't know much about plastic. Plastic materials can be divided into three categories: engineering plastics, general plastics, thermoplastic elastomer plastic materials. Engineering plastics: PC, PC/ABS, PBT, POM, PMMA, PA6, PA66, PPA, PET, PEI, PPS, PCTG, PETG, PPO, COC, LCP, PPE, etc. General plastics: ABS, PVC, EVA, PP, HIPS, HDPE, LDPE, LLD...
  • What's the reasons for dimensions NG? Jul 12, 2019
    When we do molding testing pr production, it's common to see the dimension is NG. so today we are going to discuss why the dimensions are not in tolerance. 1. Check the drawing, to see if you find the right datum? 2. Check the measuring tool, to see if it's outdated or the accuracy? or the scale is not clear, or the measuring tool not returned to zero? 3. Is the measurement method and reading corr...
  • Annealing of plastic products Jul 12, 2019
    The annealing treatment of plastic products refers to the plasticization unevenness of the plastic in the cylinder or the uneven cooling rate of the product in the cavity, which causes the internal stress of the product to cause deformation, cracking and aging of the product in the future. The annealing treatment is carried out indoors, using a hot liquid medium such as hot water, hot mineral oil,...
  • What is snake mark and how to solve it? Jul 12, 2019
    Snake mark is an indication when injection molding. So what will cause the snake mark? When injecting a plastic part, the Gate is smaller, while the space of the mold cavity is relatively larger. At this time, the temperature of resin is cooling down before it fullly injects into the whole mould cavity frame. Therefore, it will have a flowing marks remaining on the part surface like a snake crawli...
  • Learn about AS (SAN) Acrylonitrile-styrene Jul 19, 2019
    The plastic material is a solid material which is based on a polymer and is added to the additive at a certain temperature and pressure, and is formed by solidification or cross-linking. Let us learn about the material of AS now. AS is a copolymer of acrylonitrile (A) and styrene (S). It has moderate weather resistance, is not affected by high humidity environment, and is resistant to general grea...
  • What is 'Catch hook and thin-wall' of plastic mold products? Sep 18, 2019
    What is 'Catch hook and thin-wall' of plastic mold products? 1. The Catch hook The catch surface and the amount of catch hook are the important basis for the test data during assembe. Once made any tiny mistake about these numbers, It would become a huge mistake of the product. Therefore, during mould design, We needs to pay special attentin to the catch hook assembly and testing. 2. The thin-wall...
1 ... 10 11 12 13 14 ... 29

A total of 29 pages

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Home

Services

about

contact