Common injection molding product defects and solutions-3 Dec 13, 2019
Short shot-2
Solution:
1.Restart the machine after the injection is interrupted, the previous pieces may be scrapped.
2.Improve injection and shrink pressure.
3.Improve injection volume and injection speed. (Injection pressure must be sufficient)
4.Increase the mold temperature.
5.Increase the material temperature.
6.Clean the air-removal system of the mold.
7.Check if the pad is sufficient.
8.Adjust the appropriate holding pressure switching point (filling to 95% -99%).

9.Check if the gate and nozzle are blocked.